University of Colorado Boulder combines Raman spectroscopy and nanoindentation for improved materials characterisation

The University of Colorado Boulder, USA, combines Raman spectroscopy and nanoindentation for improved materials characterisation.

The Biomechanics and Biomimetics Research Laboratory at the University of Colorado Boulder uses a Renishaw inVia confocal Raman microscope to characterise biological tissues and biomaterials. The system has been interfaced with a nanoindentation system from Hysitron Inc., Minneapolis, USA, to provide combined chemical and mechanical information on samples.

Professor Virginia (Ginger) Ferguson is an Associate Professor of Mechanical Engineering at the University of Colorado who focuses on the mechanical behaviour, and underlying materials science, of biological tissues and biomaterials. Her group investigates the local mechanical properties of materials that are biological, biomimetic or used in biological tissue replacement (e.g. for tissue repair and regeneration), correlating these properties with chemical and structural information obtained from Raman and other techniques.

More specifically, Professor Ferguson's research emphasises: the experimental study and finite element modelling of native osteochondral (bone-cartilage) tissues and of materials for osteochondral tissue regeneration; bone tissue properties in mouse models that are affected by unloading and microgravity, aging, and/or metabolic disease (e.g. kidney disease); and tissues involved in successful pregnancy outcomes in humans (e.g., the cervix and chorioamnion-the ‘amniotic sac’).

The group has developed protocols and analytical solutions to collect and evaluate nanomechanical property measurements of bone, calcified cartilage and soft tissues (e.g. cartilage). They also evaluate collagen fibril orientation and alignment using secondary harmonic generation imaging and evaluate mineral volume fraction in mineralized tissues using quantitative backscattered electron imaging. The team collaborates with other groups to test materials for a wide range of engineering applications including materials for batteries/energy storage, microelectro-mechanical systems (MEMS) devices, advanced polymers and other complex material systems which makes it a varied and interesting laboratory to work in.

Pairing Renishaw's inVia™ Raman microscope with the TriboIndenter from Hysitron results in a combined instrument that provides a greatly enhanced characterisation capability complementing existing spectroscopies. Professor Ferguson said, “This unique system provides the capability to investigate mechanical properties and mechanical behaviours in parallel with imaging the chemical constituents within the materials being tested at exactly matched sites / locations with ~1 µm resolution. We use the information on a material's chemistry to elucidate changes in mechanical properties or to explain mechanical properties within single sites or when mapping over 2D regions. Moreover, mapping reveals gradients or heterogeneity of material chemistry and crystal structure. We can also uniquely evaluate chemical changes that occur following pressure induced phase transformations (that could be applied by nanoindentation, for example).”

Professor Ferguson continued, “The inVia offers a degree of customization that is not available on other systems. More importantly, we like the manner in which the inVia collects Raman spectra compared to other systems. We are the first to have joined the Hysitron nanoindenter with any Raman spectroscopy tool and have had technical challenges to overcome. I have been exceptionally pleased with the level of customer support we have received from Renishaw during the development of our unique combined instrument. Renishaw has been fantastic to work with.”

Further information on the work of the group may be found at Professor Ferguson's web site – the Biomechanics and Biomimetics Laboratory. For further details of Renishaw's inVia confocal Raman microscope, please visit www.renishaw.com/invia.

About Renishaw

Renishaw is one of the world's leading engineering and scientific technology companies, with expertise in precision measurement and healthcare. The company supplies products and services used in applications as diverse as jet engine and wind turbine manufacture, through to dentistry and brain surgery. It is also a world leader in the field of additive manufacturing (also referred to as 3D printing), where it is the only UK business that designs and makes industrial machines which ‘print’ parts from metal powder.

The Renishaw Group currently has more than 70 offices in 33 countries, with over 4,000 employees, of which 2,700 people are employed within the UK. The majority of the company's R&D and manufacturing is carried out in the UK and for the year ended June 2015 Renishaw achieved sales of £494.7 million of which 95% was due to exports. The company's largest markets are the USA, China, South Korea, Germany and Japan.

The Company's success has been recognised with numerous international awards, including eighteen Queen's Awards recognising achievements in technology, export and innovation. Renishaw received a Queen's Award for Enterprise 2014, in the Innovations category, for the continuous development of the inVia confocal Raman microscope.

Citations

Please use one of the following formats to cite this article in your essay, paper or report:

  • APA

    Renishaw plc - Spectroscopy. (2024, July 26). University of Colorado Boulder combines Raman spectroscopy and nanoindentation for improved materials characterisation. News-Medical. Retrieved on February 11, 2026 from https://www.news-medical.net/news/20160516/University-of-Colorado-Boulder-combines-Raman-spectroscopy-and-nanoindentation-for-improved-materials-characterisation.aspx.

  • MLA

    Renishaw plc - Spectroscopy. "University of Colorado Boulder combines Raman spectroscopy and nanoindentation for improved materials characterisation". News-Medical. 11 February 2026. <https://www.news-medical.net/news/20160516/University-of-Colorado-Boulder-combines-Raman-spectroscopy-and-nanoindentation-for-improved-materials-characterisation.aspx>.

  • Chicago

    Renishaw plc - Spectroscopy. "University of Colorado Boulder combines Raman spectroscopy and nanoindentation for improved materials characterisation". News-Medical. https://www.news-medical.net/news/20160516/University-of-Colorado-Boulder-combines-Raman-spectroscopy-and-nanoindentation-for-improved-materials-characterisation.aspx. (accessed February 11, 2026).

  • Harvard

    Renishaw plc - Spectroscopy. 2024. University of Colorado Boulder combines Raman spectroscopy and nanoindentation for improved materials characterisation. News-Medical, viewed 11 February 2026, https://www.news-medical.net/news/20160516/University-of-Colorado-Boulder-combines-Raman-spectroscopy-and-nanoindentation-for-improved-materials-characterisation.aspx.

Comments

The opinions expressed here are the views of the writer and do not necessarily reflect the views and opinions of News Medical.
Post a new comment
Post

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.

You might also like...
Showcase of Renishaw’s Additive-manufacture for Design-led Efficient Patient Treatment software